    With more than 10 years experiences in the industry, Tencan has accumulated a large number of application cases reports which were verified with grinding cases of various kinds of materials.We prepared some following reports for representative materials such as minerals, metal, non-metal, ceramics, chemical materials, medicine and so on. You may download.them for your references
    Green tea grinding for 70 min by planetary ball mill with corundum jars    [91]

    Vertical planetary grinding mill, 250 ml corundum tank with 250 grams of zirconium ball, dry grinding, 500 revolutions per minute, 15 grams of materials, 110 grams of large balls, 70 grams in the ball, 70 grams of small balls.

    Silica dry grinding for 90 min by planetary ball mill with zirconia jars.    [81]

    Vertical planetary ball milling, 250 ml zirconium cans with 250 grams of ball, dry grinding, 500 rpm, 5 to stop 1, 60 grams of materials, ball ratio: 25 grams of large balls, 125 grams in the ball, 100 grams of balls

    Coal dry grinding for 5 hour by planetary ball mill    [74]

    Vertical planetary grinding machine, 250 ml stainless steel tank with 370 grams of ball, dry grinding, materials 60 grams, 450 revolutions per minute, turn 5 stop 1, big ball 75 grams, 185 grams in ball, ball 110 grams

    Dinas rock grinding for 150 min by planetary ball mill    [71]

    Vertical planetary ball mill, 250 ml corundum tank with zirconium ball 280 grams, 480 revolutions per minute, turn 5 stop 1, dry grinding, 50 grams of materials, big ball 30 grams, 250 grams in the ball, 30 grams of star ball

    Black lead wet grinding for 4 hours by planetary ball mill+zirconia jars    [72]

    Vertical planetary ball milling, 250 ml zirconium cans, Peng 50 grams of zirconium ball, wet grinding, 450 rpm, 5 to stop 1, 50 grams of materials, 50 grams of water, 0.4 grams of dispersant, ball ratio: 200 grams of small balls, big ball 50 grams

    Gaolin clay wet grinding with corundum jar    [63]
    Vertical planetary ball mill, 250 ml corundum tank with 300 grams of zirconium ball, wet grinding, 450 rpm, 5 to stop 1, 15 grams of materials, 100 grams of water, 150 grams of small balls, 100 grams in the ball, big ball 50 grams.


    Rare earth oxide grinding for 2 hours with zirconia jars and ethyl alcohol    [65]
    Vertical planetary grinding machine, 250 ml zirconium cans with 250 grams of zirconium ball, wet grinding, 450 revolutions per minute, 50 grams of materials, water 50 ml, ball ratio: big ball 50 grams, 100 grams in the ball, 100 grams of balls.
    Valcanic rock grinding for 18 hours by stir ball mill    [102]
    Stir ball mill, 1 liter stainless steel tank and 1000 grams of 3 mm ball, add 200 grams of water, 300 grams of material, 400 rpm.
    Valcanic rock grinding for 2 hours by stir ball mill    [69]
    Silver sand grinding for 16 hours by planetary ball mill with zirconia jars    [64]
    Titanium pigment wet grinding for 10 hours by planetary ball mill    [69]
    Fe3O4 dry grinding for 5.5 hours    [68]
    Please Feel free to give your inquiry in the form below.We will reply you in 24 hours.
     * *
     *
     *
     验证码,看不清楚?请点击刷新验证码  
         |   Home    |    Products      |      Model Selection      |      Services Online      |      About Us      |      Contact Us      |        
       
     
           
     
    sales@lab-mills.com
    service@lab-mills.com
    0086-13357214760
    0086-731-84939972
    0086-731-84939973